镀镍:打底用,增进抗蚀能力。
PH value too high or low, general nickel plating or gold-plated (low won ) is happening.PH值过高或过低,一般镀镍或镀金(过低不会)皆会发生。
A method for continuous titration of boric acid and nickel chloride in bright nickel plating bath was presented.介绍了一种光亮镀镍液中硼酸和氯化镍的测定方法。